Standard Clay Company
Plastic clay for wheel and modeling. Granular manganese gives speckled surface. Ideal temperature for best color is C/5. Good in oxidation or reduction firing. Contains manganese.
C/4 Average Shrinkage 10.5% Absorption 4.5%
C/6 Average Shrinkage 11.0% Absorption 2.25%
All sales final. Pickup at our studio: 753 NE 79 St Unit 761, Miami, FL 33138.
Standard Clay Company
Plastic clay for wheel and modeling. Granular manganese gives speckled surface. Ideal temperature for best color is C/5. Good in oxidation or reduction firing. Contains manganese.
C/4 Average Shrinkage 10.5% Absorption 4.5%
C/6 Average Shrinkage 11.0% Absorption 2.25%
All sales final. Pickup at our studio: 753 NE 79 St Unit 761, Miami, FL 33138.